Abstract:A series of three-layer polyimide films with sandwich-like structure were prepared by coating polyamic acid onto both sides of middle-layer polyimide and further thermal imidization. The middle-layer polyimide came from the condensation of 3,3′,4,4′-biphenyltetracarboxylic dianhydride(BPDA) and p-phenylenediamine(PDA) /4,4′-oxydianiline(ODA), and the top and bottom layers were the thermoplastic polyimide made from the polymerization of BPDA and 2,2′-bis[4-(4-aminophenoxy)phenyl] propan(BAPP). In order to improve the toughness of three-layer polyimide films, poly(MIPOSS-alt-NA) was introduced into the top and bottom layers. It is found that the elongation at break of the three-layer polyimide film increases from 7.2% to 14.5% and the coefficient of thermal expansion (CTE) decreases from 27.0×10-6K-1 to 23.6×10-6K-1 with 6.0% poly(MIPOSS-alt-NA). Furthermore, the peel strength of flexible copper clad laminate (FCCL) made with the three-layer polyimide film achieves 12.0 N/cm. The toughening mechanism was investigated by SEM micrographs of tensile-fractured surface.