Abstract:Polyvinyl alcohol (PVA) hydrogel membranes have transport properties due to cross-linked network structure. It is of considerable significance to regulate the permeation and diffusion behavior of ions through mesh size for selective permeation functions. In this paper, glutaraldehyde was used as cross-linking agent to prepare PVA hydrogel membranes with different mesh sizes, and the permeability of ions in the hydrogel membrane was studied. Fourier transform infrared spectrum(FT-IR), X-ray diffraction (XRD) and scanning electron microscopy (SEM) were used to characterize the microstructure of the PVA hydrogel membrane, and calculate gel contents, swelling degrees and mesh sizes. These parameters were related to the permeability of ions in the PVA hydrogel membranes. The results show that as the concentration of the cross-linking agent increases, the degree of cross-linking of the PVA hydrogel membrane increases, the mesh size decreases accordingly, and the crystallinity and swelling properties also decrease significantly. At the same time, when the mesh size is adjusted from 15.07 nm to 3.76 nm, the permeability coefficients of K+, Na+, Ca2+, and Mg2+ also fall from 19.5×10-7 cm2/s, 18.0×10-7 cm2/s, 12.2×10-7 cm2/s, and 10.9×10-7 cm2/s to 3.44×10-7 cm2/s, 2.84×10-7 cm2/s, 2.22×10-7 cm2/s, and 1.76×10-7 cm2/s, which realize the regulation of ion permeation behaviors by these crosslinked PVA hydrogel membranes.