Abstract:Flowable Eucommia ulmoides gums(EUG) with aldehyde and ketone end group were prepared by indirect oxidation method. First, Epoxidized Eucommia ulmoides gums(EEUG) were prepared via emulsion process, and then EEUG was oxidized and degraded with periodic acid. The effects of the degree of epoxidation, reaction time and amount of periodic acid on the molecular weight and its distribution of LEEUG were studied by 1H-NMR and GPC. Also, the structure and properties of LEEUG were measured by IR, 13C-NMR, DSC and TG. The results show that the number average molecular weight of the obtained liquid Eucommia ulmoides gum ranges form 8000 to10000 under the optimal experimental conditions of oxidative degradation. Periodic acid breaks the chains by attacking epoxy group rather than carbon carbon double bond. The degree of epoxidation shows little effect on the molecular weight of LEEUG, but the crystallinity of LEEUG can be controlled by regulating the degree of epoxidation. Compared with EUG and EEUG, the thermal degradation temperature of LEEUG is increased by 56 ℃. The molecular weight and molecular weight distribution of liquid Eucommia ulmoides gums have a significant effect on the rheological behavior. The higher the number average molecular weight and the narrower the molecular weight distribution,the greater the complex viscosity of LEEUG.