Abstract:In order to study the preparation process and electrical properties of polypropylene (PP), 4-acetoxystyrene (AOS) was grafted onto PP by melting method. The effects of preparation process on the grafting rate and the effects of grafting rate on space charge and dielectric properties were studied. The results show that when the mass of PP is 50 g, the amount of dicumyl peroxide (DCP) changes the grafting rate of the product. When the dosage of DCP is 0.12 g, the grafting rate increases gradually with the increase of AOS dosage, and then becomes stabilized. However, when the dosage of DCP is 0.04 g and 0.08 g, the AOS dosage increases first, and then decreases. With the increase of temperature, rotation speed and time, the grafting rate first increases and then decreases. Therefore, the optimum process of PP-g-AOS grafting material is m(PP)∶m(AOS)∶m(DCP)= 50∶1.4∶0.08, temperature of 190 ℃, speed of 80 r/min, time of 8 min, the graft rate is 1.14%. With the increase of grafting rate, the abilities of the grafted product to suppress the internal space charge, the breakdown strength and the volume resistivity first increase and then decrease, while the dielectric constant and dielectric loss do not change much; when the grafting ratio is 1.14%, the electrical properties of the grafted materials are the best. At this time, the PP-g-AOS grafting material has the best effect of suppressing space charge, the volume resistivity is 5.1×1015 Ω·m, which is 3.25 times higher than that of pure PP, and the breakdown strength is 48.7 kV/mm, which is twice that of pure PP. It lays a solid theoretical and practical foundation for the study of non-crosslinked polypropylene cable insulation materials with high electrical properties.