    摘要:

    采用共沉淀法分别制备出水滑石(Zn-Mg-Al-LDHs)与含稀土元素La改性水滑石(Zn-Mg-Al-La-LDHs)阻燃剂样品,通过X射线衍射、能谱仪对阻燃剂样品进行表征。利用热重分析、氧指数和锥形量热等研究了水滑石及含稀土元素La改性水滑石对硅橡胶泡沫材料(SRF)阻燃及抑烟性能的影响。结果表明,Zn-Mg-Al-LDHs和Zn-Mg-Al-La-LDHs被成功制备,将两者添加到SRF中,垂直燃烧等级均达到V-0级别,添加量为20%(质量分数)的Zn-Mg-Al-La-LDHs/SRF的极限氧指数(LOI)可达32.8%。改性前后SRF燃烧残余物表面形成致密保护炭层,其中添加量为5%(质量分数)的Zn-Mg-Al-La-LDHs/SRF的炭层更加致密。与未添加阻燃剂的SRF相比,含5%Zn-Mg-Al-La-LDHs/SRF的热释放速率峰值(PHRR)和烟释放率峰值(PSPR)分别降低了56.53%和59.52%。Zn-Mg-Al-LDHs与Zn-Mg-Al-La-LDHs均提高了SRF的热稳定性,当两者添加量为5%,SRF材料的残余炭渣率分别提升了15.69%和10.84%。

    Abstract:

    The flame retardant samples of hydrotalcite (Zn-Mg-Al-LDHs) and rare earth-containing La-modified hydrotalcite (Zn-Mg-Al-La-LDHs) flame retardant were prepared by coprecipitation method.The characteristics were analyzed by XRD and SEM-EDS. The simultaneous thermal analyzer, limit oxygen index and the cone calorimeter test were adopted to learn the effects of hydrotalcite and rare earth-containing La-modified hydrotalcite flame retardants on the flame retardancy and smoke suppression performance of silicone rubber foam (SRF). The result show that Zn-Mg-Al-LDHs and Zn-Mg-Al-La-LDHs have been successfully producted. Furthermore, by adding both to SRF, the vertical combustion grades reach to the V-0 level. When the addition amount raises to 20%, the limiting oxygen index (LOI) of Zn-Mg-Al-La-LDHs/SRF is up to 32.8%. A dense protective carbon layer is formed on the surface of the SRF combustion residue before and after the modification. In particular, the carbon layer of 5%-added Zn-Mg-Al-La-LDHs/SRF is denser. Compared to SRF without flame retardant, the peak of heat release rate (PHRR) and smoke release rate (PSPR) with added 5% Zn-Mg-Al-La-LDHs are reduced by 56.5% and 59.5%, respectively. Both Zn-Mg-Al-LDHs and Zn-Mg-Al-La-LDHs improve the thermal stability of SRF. When the mass fraction of both is 5%, the rate of residual carbon residue of the SRF is increased by 15.69% and 10.84%, respectively.

    参考文献
    相似文献
    引证文献
引用本文

马 砺, 刘西西, 刘志超, 康付如, 魏 泽.改性水滑石的制备及在硅橡胶泡沫阻燃抑烟中的应用[J].高分子材料科学与工程,2020,36(10):55-62. Li Ma, Xixi Liu, Zhichao Liu, Furu Kang, Ze Wei. Preparation of Modified Hydrotalcite and Its Application in Flame Retardant and Smoke Suppression of Silicone Rubber Foam[J]. Polymer Materials Science & Engineering,2020,36(10):55-62.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2020-12-15
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司