Abstract:Polyamide-imide (PAI) composite coatings with SiC and polytetrafluoroethylene (PTFE) as filler were deposited on Q235 stainless steel substrates by spraying technique at room temperature, and their friction and wear behavior were investigated through MMW-1 universal frictional wear testing machine. Tribological performance of PAI composite coatings reaches to the best, SiC and PTFE mass fraction are 10% and 0.8%, respectively. For pure PAI and the PAI+10%SiC coating, under an applied load of 40 N, the increase in sliding velocity can result in the decreasing of friction coefficient at a cost of wear resistance. However, under an applied load of 120 N, the coatings show the highest friction coefficient and wear rate at the low and intermediate velocity. For the SiC+10%SiC+0.8%PTFE coating, the friction coefficient gradually decreases with the increase of load due to PTFE filled, while the wear rate increases firstly and then remains basically unchanged. Moreover, the increase of sliding velocity only leads to the decrease of friction coefficient and wear rate. TG curves reveal that the initial decomposition temperature of the composite coatings is 410 ℃, while that of the pure PAI coatings is 350 ℃. SEM micrographs of the worn coatings reveal the wear mechanism, pure PAI coating is abrasive wear, SiC/PAI composite coatings are ploughing wear, and SiC/PTFE/PAI composite coatings only show slight plastic deformation.