    摘要:

    采用溶液聚合法合成了以聚四氢呋喃(PTMG)为软段、4,4’-偶氮苯二甲酸(Azoba)和六亚甲基二异氰酸酯(HDI)为硬段、双(2-羟基乙基)二硫醚(HEDS)为扩链剂的不同硬段比例的形状记忆聚氨酯(SMPUs)。红外光谱表征了聚氨酯薄膜化学结构;分别通过热重分析、差示扫描量热分析、动态力学分析(DMA)探究了硬段对聚氨酯材料热稳定性、熔融温度及形状记忆性能的影响;记录了SMPU2在紫外光照刺激下响应、发生形变的过程;用划痕修复测试和接触角法表征自愈合能力。结果表明,调控软硬段比例可得到具有差异形状记忆性能的SMPUs。DMA测试中SMPUs的平均固定率高于75%,回复率均高于95%,其中硬段含量为44%的SMPU2形状记忆性能最佳,固定率达91%,回复率达99%。引入含双硫键的单体,SMPUs具有一定自愈合性能。其中SMPU5在40 ℃修复30 min,能修复表面划痕,力学测试表征的修复性能在60 ℃修复120 min修复率可达90%。

    Abstract:

    Shape memory polyurethanes(SMPUs), with polytetrahydrofuran(PTMG)as soft segment, 4,4'-azobisbenzoic acid(Azoba)and hexamethylene diisocyanate(HDI)as hard segment, and bis(2-hydroxyethyl)disulfide(HEDS)as chain extender were synthesized via solution polymerization. The chemical structures were studied by FT-IR and 1H-NMR. The effects of hard segment contents on the thermal stability, melting temperature(Tm)and shape memory properties of polyurethane materials were investigated by thermogravimetric analysis(TG), differential scanning calorimetry(DSC)and dynamic mechanical analysis(DMA)of thermal cyclic tension. A camera was used to record the deformation of SMPU2 in response to UV light stimulation. Self-healing abilities were characterized via change in contact angle and the scratch recovery tests. The results indicate that the difference in shape memory performance of SMPUs is due to regulating the content of hard segments. Meanwhile, SMPUs exhibit good shape memory properties with higher than 75% fixity ratio and the 95% recovery ratio via DMA tests. SMPU2(hard segment content of 44%)shows excellent shape memory performance with fixity ratio(91%)and recovery ratio(99%). More importantly, surface scratches of the SMPU5 can be repaired within 30 min at 40 ℃ and tensile tests show the repair rate is up to 90% in 120 min at 60 ℃ because of the existence of disulfide bonds.

    参考文献
    相似文献
    引证文献
引用本文

李佩杰, 万里鹰.可自愈合的紫外光响应形状记忆聚氨酯的制备及性能[J].高分子材料科学与工程,2021,37(5):93-101. Peijie Li, Liying Wan. Preparation and Properties of UV Light-Trigger Deformation Shape Memory Polyurethane with Self-Healing[J]. Polymer Materials Science & Engineering,2021,37(5):93-101.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2021-08-06
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司