Abstract:Based on the melt blending method, a twin-rotor continuous mixing extruder was used to prepare polylactic acid (PLA)/polycaprolactone (PCL) degradable blends, and the effect of PCL content and rotor speed on the properties of blends was studied. Tensile test, dynamic mechanical analysis, thermogravimetric analysis, differential scanning calorimetry analysis and other tests were applied to investigate the mechanical properties, thermal stability and crystallization properties of PLA/PCL blends. The results show that PCL has a significant toughening effect on PLA/PCL blends, and can improve the thermal stability and crystallization properties of the blends. Increasing the rotor speed can improve the dispersion and distribution of the dispersed phase in the continuous phase, but too high speed will cause the thermal degradation of PLA and the aggravated cracking of PCL. When the rotor speed is 500 r/min and PCL mass fraction is 40% or 50%, the PLA / PCL blends have good comprehensive properties. At this case, the tensile strength is higher than 48 MPa, the elongation at break is higher than 466%, the impact strength is higher than 82 J/m, the crystallinity of PCL phase and PLA phase is higher than 56.08% and 52.90% respectively.