Abstract:It is difficult to estimate the lifetime of commercial rubber products through traditional mechanical properties due to small size and abnormal shape. To solve this problem, the oxidation induction time (OIT) was used as performance change index to predict the life of EPDM O-rings for the first time. The EPDM O-rings were subjected to accelerated thermal aging at 80 ℃, 100 ℃, 120 ℃, 140 ℃ and 160 ℃ for several hours to two years, and the samples before and after aging were tested for tensile strength, elongation at break and oxidation induction time. The research results show that, with the extension of aging time and increase of aging temperature, the change trend of the oxidation induction time is consistent with the tensile strength and elongation at break. And the lifetime of EPDM O-rings calculated with OIT as performance change index is 28.6 years, which is almost the same as the tensile strength as performance change index. It proves the feasibility of using OIT as performance change index for life estimation, and the problem of life estimation for small-sized and special-shaped products can be solved.