Abstract:Poly(vinylidene fluoride) (PVDF) microporous membranes were fabricated via melt extrusion-stretching method (MES) using high and low molecular weight PVDF mixture as raw material. The effect of hot-stretching temperature during hot-stretch step on the surface morphology and crystallization behavior of PVDF microporous membranes were investigated by SEM, FT-IR, XRD, differential scanning calorimetry (DSC) and so on. The results indicate that hot-stretching temperature has profound influences on the pore morphology, porosity, crystallinity and content of β phase. When the stretching temperature is 80 ℃, the crystallinity of microporous membranes is 58.86%, and the relative content of β phase increases to 42.50%, the microporous membranes exhibit the best mechanical properties. When the stretching temperature rises to 120 ℃, the amount and uniformity of pores are greatly improved. The porosity of microporous membrane can reach as high as 31.51%.