Degradation Properties of Magnesium-Polycaprolactone Composite by Fused Extrusion Additive Manufacturing Process
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为了解决聚己内酯(PCL)在骨修复领域存在的力学性能不足、降解时间过长、表面疏水和骨诱导性不足的问题,文中通过在PCL基底内引入镁(Mg)粉末颗粒,采用溶液共混的方式,制备了Mg/PCL复合材料。采用熔融挤出增材制造技术制造了用于骨修复的多孔支架。设计了体外降解实验,从降解液的pH可以看出,Mg/PCL 的pH升高,纯PCL的pH降低,说明复合材料降解产生了碱性物质;从结晶度和压缩强度测试结果可以看出,Mg颗粒的加入降低了纯PCL的结晶度和压缩强度;通过观察多孔支架的微观形貌,可以看到Mg/PCL多孔支架表面附着的Mg颗粒随着降解时间的延长逐渐脱落,支架表面形成了更为明显的降解裂纹;测量了降解后2种材料的相对分子质量,其中Mg/PCL复合材料的相对分子质量下降更为明显。结果表明,Mg颗粒的加入,加快了PCL的降解速度,降解产生的Mg离子对骨缺损部位的修复有促进作用。通过实验结果可知,与其他生物材料相比,改变Mg/PCL复合植入物中Mg的含量,能够调控PCL的降解速度,使降解过程与骨再生过程相匹配,在骨软骨领域有着良好的应用前景。

    Abstract:

    As bone repairation biomaterial, polycaprolactone has disadvantages of poor mechanical properties, long degradation time, hydrophobic surface and poor osteoinductive property. Mg micro-particles were incorporated into the PCL matrix to produce Mg/PCL composite materials and fused extrusion additive manufacture technology was used to fabricate bone repair porous scaffolds. By the vitro degradation experiment, from the pH of the degradation solutions, the result shows that the pH of Mg / PCL increases and the pH of pure PCL decreases, which indicates the degradation of the composite and alkaline substances were produced. From the crystallinity and compressive strength test results, it can be seen that the addition of Mg particles reduces the crystallinity and compressive strength of pure PCL. By observing the micro morphologies of porous scaffolds, Mg particles attached to the surface of Mg / PCL porous scaffolds gradually fall off with the increase of degradation time, and more obvious degradation cracks are formed on the surface of scaffolds. The molecular weight of the two materials after degradation was measured. The molecular weight of Mg/PCL composite decreases more obviously. The results show that the addition of Mg particles accelerates the degradation rate of PCL, and the Mg ions produced by degradation promote the repair of bone defects. The experimental results show that compared with other biomaterials, changing the content of Mg in composite implants can regulate the degradation rate of PCL and match the degradation process with the bone regeneration process, which has good application prospects in the field of osteochondral.

    参考文献
    相似文献
    引证文献
引用本文

刘永财, 伍言龙, 刘亚雄.熔融挤出增材制造的镁/聚己内酯复合材料的体外降解特性[J].高分子材料科学与工程,2021,37(11):125-133. Yongcai Liu, Yanlong Wu, Yaxiong Liu. Degradation Properties of Magnesium-Polycaprolactone Composite by Fused Extrusion Additive Manufacturing Process[J]. Polymer Materials Science & Engineering,2021,37(11):125-133.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2022-03-02
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司