Abstract:Poly (L-lactide) acid/cellulose acetate three-dimensional micro-nanofibrous porous scaffolds were prepared by low-temperature quenching, extraction, washing and drying using N, N-dimethylformamide, tetrahydrofuran, acetonitrile, 1, 4-dioxane and N, N-dimethylacetamide as solvent respectively, without the assistance of other additives. The experimental results show that the three-dimensional micro-nanofibrous porous structure with the diameter of 50~350 nm was obtained using tetrahydrofuran as solvent, which has the same size and structure as the natural extracellular matrix (50~500 nm). The effects of quenching time, quenching temperature, polymer concentration and PLLA/CA mass ratio etc. on the morphologies of fibrous scaffolds were investigated by SEM. The influence of the addition of CA on the hydrophilicity, mechanical properties and biological activity of fibrous scaffolds were investigated by water contact angle, water absorption, mechanical properties and in vitro biological activity tests. The experimental results show that, compared with pure PLLA fibrous scaffold, the addition of CA improves the hydrophilicity, compressive strength and impact strength of PLLA/CA three-dimensional micro-nanofibrous porous scaffolds, and then enhances the biological activity of the materials. The porosity and specific surface areas of PLLA/CA three-dimensional micro-nanofibrous porous scaffolds are all greater than 94% and 52 m2/g respectively, indicating that PLLA/CA three-dimensional micro-nanofibrous porous scaffolds are three-dimensional porous materials with high porosity and large specific surface area, which will offer good conditions for cell adhesion, cell differentiation, cell prolifer and nutrients transport.