Abstract:A series of polycaprolactone (PCL) shape memory materials with different photoinitiator contents were prepared. The PCL was crosslinked through a thermal initiator to initiate the free radical combining with the synergistic effect of secondary curing on the surface of ultraviolet light. The effects of Irgacure 2959 (Ir2959) on the crystallinity, thermal stability, mechanical properties, and shape memory properties of PCL cross-linked materials were investigated. The relationship between the structure and shape memory properties was investigated by differential scanning calorimetry (DSC), thermogravimetry (TG), shape memory performance and mechanical performance testing. The results show that, compared with the thermal cross-linking system, the UV light surface secondary curing enhances the shape memory performance and mechanical properties of the materials significantly. When the photoinitiator Ir2959 is added up to 3% (P/B/I-3), the shape memory performance of the material reaches the highest. The shape fixation rate (Rf) and shape recovery rate (Rr) of P/B/I-3 sample are increased from 93.0% and 91.4% to 99.5% and 99.8%, respectively. The tensile strength and elongation at break of P/B/I-3 sample are increased from 42.5 MPa and 658.1% to 49.9 MPa and 805.0%, respectively.