Abstract:A series of high-strength wood membranes were prepared by removing matrix from balsa wood first, and then applying 2,2,6,6-tetramethylpiperidinooxy (TEMPO) oxidation and acetylation on the cellulosic wood skeletons. The effects of above chemical treatments on mechanical properties, optical performance, morphology, surface characteristics and crystalline structure of the wood membranes were investigated systematically. The results show that after removing matrix, the obtained cellulosic wood skeletons could be converted into a dense wood membrane with layer structures under drying conditions. The density of this wood membrane is almost five times higher than that of the original wood. Further, TEMPO oxidation and acetylation treatments on cellulosic wood skeleton contribute to significantly improved optical and mechanical properties for the wood membranes. For example, the TEMPO oxidized wood membrane shows a light transmittance as high as 61.8% and fracture tensile stress of 180.29 MPa. For acetylated wood membrane, it has an excellent tensile strength of 264.14 MPa, which is almost 14 times higher than the original balsa wood. This acetylated wood membrane is further utilized as flexible substrate to develop an intelligent anti-counterfeiting label. Generally, these research results can provide theoretical basis and technical support for the promotion of high-value utilization of wood resources.