    摘要:

    以4,4’- 双马来酰亚胺二苯甲烷(BMI-1)、双酚A型氰酸酯(BADCy)和酚酞型聚芳醚砜(PES-C)为原料通过加入发泡剂合成了双马来酰亚胺/氰酸酯耐高温发泡胶。通过差示扫描量热分析和红外表征分析了树脂的固化行为。扫描电子显微镜分析表明,该发泡胶发泡均匀细腻(平均泡孔直径0.275 mm)。热重分析结果表明,该发泡胶具有很高的耐温性:空气和氮气氛围下10%分解温度分别为393 ℃和412 ℃。发泡胶在9.375 GHz频率下的介电常数为1.65、介电损耗为0.0057,展现了优异的介电性能。管剪测试表明,该发泡胶具有优异的黏结性能和耐温性能,-55 ℃、25 ℃和150 ℃管剪强度均大于7 MPa,205 ℃管剪强度不小于4 MPa。与多种材料的拉伸测试结果表明,该发泡胶与多种材料具有优异的黏结性能,铝-铝拉伸强度为9.2 MPa、钛-钛拉伸强度为5.9 MPa、双马基复材-双马基复材拉伸强度为5.9 MPa。

    Abstract:

    A high temperature resistant bismaleimide/cyanate foam adhesive was synthesized with 4,4’ - bismaleimide diphenylmethane (BMI-1), bisphenol A dicyanate (BADCy), phenolphthalein polyaryl ether sulfone (PES- C) and blowing agent. The cure reaction of the resin was investigated by differential scanning calorimetry (DSC), in situ FT-IR. SEM analysis suggest the foam evenly with fine cells, the average cell diameter is 0.275 mm. Thermogravimetric analyzer (TGA) suggests that the foam adhesive has a higher temperature resistance, Td10 in air and nitrogen atmosphere is 393 ℃ and 412 ℃, respectively. At 9.375 GHz, the dielectric constant of foam is 1.65, tan δ is 0.0057, showing excellent dielectric properties. Pipe shear test shows that it has excellent bonding performance and the temperature resistance -55 ℃, 25 ℃ and 150 ℃ pipe shear strength is not less 7 MPa, 205 ℃ pipe shear strength is greater than 4 MPa. Tensile test of the foam adhesive with a variety of materials shows that ithas excellent bonding properties to a variety of materials, aluminum- aluminum tensile strength is 9.2 MPa, titanium-titanium tensile strength is 5.9 MPa, bismaleimide composite material- bismaleimide composite material strength is 5.9 MPa.

    参考文献
    相似文献
    引证文献
引用本文

赵道翔,李 刚,宋军军,陈维君,崔宝军.双马来酰亚胺/氰酸酯型发泡胶的制备与表征[J].高分子材料科学与工程,2022,38(4):126-133. Daoxiang Zhao, Gang Li, Junjun Song, Weijun Chen, Baojun Cui. Preparation and Characterization of Bismaleimide Foam Adhesive[J]. Polymer Materials Science & Engineering,2022,38(4):126-133.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2022-07-23
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司