Abstract:GO with a large layer spacing was prepared to make the path of corrosion medium invading steel substrate become zigzag and the time become longer, and to enhance the density and adhesion of water- based epoxy coating. First of all, Gamma-aminopropyl triethoxysilane (KH550) was hydrolyzed to synthesize aminocagetype sesquisiloxane (POSS-NH2); secondly, the self- polymerization advantage of mussel inspired dopamine was utilized to reduce and functionalize GO. The reduction and functionalization of GO can be easily achieved by the oxidative polymerization of dopamine at room temperature and under weakly alkaline (pH=8.5) conditions. The resulting polydopamine was coated on GO sheet and provided rich amine groups and carbonyl groups to achieve functionalization. Finally,PGO-POSS was prepared by Schiff base reaction between the amino groups of POSS-NH2 and carbonyl groups of PGO under alkaline condition, which was used to prepare the waterborne epoxy anticorrosive coating. The structure of the product was confirmed by Fourier-transformed infrared spectrum(FTIR), X- ray photoelectron spectroscopy(XPS), X- ray crystal diffraction test(XRD)and ultra- high resolution scanning electron microscope(SEM), POSS- NH2 was successfully grafted onto the surface of PGO. The anticorrosive properties of waterborne epoxy coating were measured by electrochemical and salt spray experiment. The results show that when 1% PGO-POSS was added (the addition amount is based on the total mass of epoxy resin and curing agent, the same below), the best corrosion resistance is got, and the corrosion inhibition efficiency can reach 99.72%. Compared with pure EP, the corrosion current density is reduced from 112202 nA/cm2 to 316 nA/cm2, the corrosion voltage is increased from - 0.58 V to - 0.17 V, and the low- frequency impedance value is increased by about four orders of magnitude. The coating is expected to enhance the long-term corrosion resistance of steel matrix.