Abstract:The blends of siloxane modified epoxy resin and phenolic resin have good heat resistance and toughness. The focus of structural and composition evolution of the blends under the condition of hot oxygen is of great significance to broaden the application fields of phenolic resin at high temperature. In this study, modified epoxy (ES) was synthesized by the condensation of hydroxy-terminated polydimethylsiloxane (HTPDMS) and epoxy resin, which is blended with phenolic resin to obtain polysiloxane modified epoxy/phenolic blends (ES/PF). The thermal properties of ES/PF blends and chemical structure after pyrolysis were investigated by thermogravimetric analysis (TGA), FT-IR, scanning electron microscope additional energy dispersive spectrometer (SEM-EDS) and Xray photoelectron spectroscopy (XPS). Thermal analysis results reveal that compared with phenolic resin, the residual rate of ES/PF blends is increased by 438% at 800 ℃ under air condition, the maximum exothermic rate is decreased from 21.98 mW/mg to 14.93 mW/mg, and the residual rate is decreased by 14.3% in N2. Combined with infrared analysis, the hybrid structure Si—Ox formed by ES/PF pyrolysis at 430~600 ℃, which can stabilize the formation of carbon layer, delay and hinder the further degradation of the resins and improve the char yield. XPS and EDS results reveal that the occurrence form of silicon element changes significantly at high temperature, and most of them change into SiO2 and SiO2·nH2O above 430 ℃. Indicating that the introduction of silicon can increase the char yield and has a positive effect on the thermal stability of phenolic resin under thermal oxygen condition, while the beneficial effect of silicon is inhibited in N2. This may be related to the oxygen absorption mechanism of siloxane group pyrolysis. The pyrolysis structure and composition of ES/PF blends are beneficial to improve the thermal residual strength and ablative resistance of the blends.