Abstract:Poly (4- hydroxybutyrate) (P4HB) is a highly promising polyhydroxyalkanoates (PHAs). Compared with biological fermentation, P4HB prepared by chemical synthesis has the advantages of adjustable molecular weight, narrow molecular weight distribution, low cost, and adjustable terminal functional groups. In this paper, P4HB monofilament sutures were prepared by melt spinning process, and the effects of primary stretching ratio, secondary stretching ratio, and secondary stretching temperature on the spinnability, mechanical properties, crystallization, orientation and surface morphology of P4HB monofilament were systematically studied by DSC,SEM,WAXD and other test methods. It is found that selecting 5 times primary stretching, 1.3 times secondary stretching and 40 ℃ secondary stretching temperature can make the P4HB monofilament suture with the best performance. In addition, the P4HB suture has stable performance under normal temperature storage conditions, and its mechanical strength can be maintained for a long time during in vitro degradation. Different specifications of P4HB sutures were prepared based on the optimized process, and their mechanical properties exceed the industry standards and existing products.