Abstract:To obtain polyimides films with better dimensional stability properties, different mole ratios of 4,4'-oxybisbenzenamine (4,4'-ODA) and 2- (3-amino-phenyl)-benzooxazol-5-ylamine (DAPBO) were used to polymerize with 3,3’,4,4’- biphenyl tetracarboxylic diandhydride (BPDA). The samples were systematically characterized, observed and measured by infrared spectrum characterization and thermal properties. Results show that the thermal stabilities and glass transition temperatures (Tg) increase with the increasing ratio of DAPBO because of the rigid structure of DAPBO. The coefficients of thermal expansion (CTE) are decreased with the increasing ratio of DAPBO. When the mole ratio of 4,4'-ODA and DAPBO is 4:6, the CTE is closed to 18×10- 6 K- 1, indicating that it is more appropriate to make flexible printed circuit boards with above-mentioned films.