Abstract:Blocked polyisocyanate crosslinker (BIC) and fluorinated polyacrylate emulsion (FPA) with different melting points and deblocking temperature were prepared. The chemical structure and microstructure of FPA were characterized by FT-IR and TEM. BFCM was obtained by hydrophobic treatment of cotton fabric with 1K emulsion FBPA composed of BIC and FPA. The static hydrophobicity, dynamic spray, contact angle, friction resistance and washing resistance of BFCM were tested. The effect of the melting point and deblocking temperature of BIC on the hydrophobicity of BFCM was compared. The results show that the waterproofing, wearresisting and washable properties of BFCM are improved significantly with the decrease of the melting point and deblocking temperature of BIC. When the melting point of BIC is 6.6 ℃, the lowest deblocking temperature of BIC is 75 ℃ , under the 110 ℃ treatment, the water contact angle(WCA) of BFCM can reach 142.9° and the hydrophobic grades can reach 5. After the treatment at 100 ℃ for 50 friction cycles and 24 h water washing, WCA can still reach 132.5° and 136.5°, respectively