Abstract:Poly(dodecamethylene terephthalamide- co- ethylene terephthalate) (poly(12T- co- ET)) copolymer was prepared by amidation reaction of dodecanediamine (DDMD) and polyethylene terephthalate (PET) with sulfolane as solvent. The effects of reaction temperature, feeding ratio, and solvent mass on the relative viscosity and conversion rate of the product were investigated, and the optimal rection conditions were determined as follows, the reaction temperature, feeding mole ratio of DDMD to PET and mass ratio of PET to solvent are 210 ° C, 1.1:1 and 1:10, respectively. Under the above conditions, the relative viscosity of the obtained product and conversion rate are 1.37 and 82.1%, respectively. The structure of the product was confirmed by Fourier transform infrared spectroscopy (FT-IR) and proton nuclear magnetic resonance spectroscopy (1H-NMR). From the results of differential scanning calorimetry (DSC) and thermal gravimetric analysis (TGA), it is found that the melting temperature, crystallization temperature and initial thermal decomposition temperature of the product are 234 °C, 201 °C and 357 °C, respectively. Besides, the tensile strength, elongation at break, bending strength and notched impact strength are 37.0 MPa, 9.32%, 49.2 MPa and 1.5 kJ/m2. And the dynamic thermomechanical analysis (DMA) show that its glass transition temperature (Tg) is 91.0 °C. In conclusion, poly(12T-co-ET) can be used as matrix resin for blending modification despite its mechanical properties is unsatisfactory, which supplies a certain reference value for the recycling of PET and environmental protection.