Abstract:To prepare eco-friendly waterborne wood coatings based on renewable material, the properties of wood coating derived from styrene grafted natural rubber latex were investigated. The results show that the pH value of the coatings does not change significantly. The viscosity is increased with the increase of the amount of styrene, and the reaction temperature has little effect on the viscosity of the coatings. When the amount of styrene increases, the drying time of the coating film is shortened, the adhesion is enhanced, and the hardness is increased. When the reaction temperature is increased, the drying time of the coating film does not change significantly, but the adhesion and hardness are improved. When the amount of styrene added is 15% and the reaction temperature is 90 ℃, the pH of the coating is 9.8, the viscosity is 310 mPa · s, the drying time of the coating film is 10 min, the adhesion reaches grade 2, and the hardness is 3B, the grafting rate is 7.1% .Fourier transform infrared spectroscopy and nuclear magnetic resonance hydrogen spectroscopy show that the graft copolymerization of styrene and natural rubber emulsion occurs, the water contact angle increases to 58.16°, and the fracture surface of the coating film is more solid and dense. Styrene can graft in the molecular structure of natural rubber, and has little effect on the properties such as appearance and viscosity of emulsion. It can enhance the physical and mechanical properties such as adhesion and hardness after the coating is formed into film, and has the potential to replace the traditional petroleum-based waterborne wood coatings.