异佛尔酮二异氰酸酯反应增容聚己二酸-对苯二甲酸丁二酯/聚乳酸生物降解阻隔膜的结构与性能
作者:
作者单位:

作者简介:

通讯作者:

中图分类号:

基金项目:

国家自然科学基金资助项目(52003036);福建省海洋经济发展专项资金项目(FJHJF-L-2022-7);厦门海洋研究开发院共建项目(KFY202203);高分子材料工程国家重点实验室开放课题基金(sklpme2022-4-02);福建省科技计划(2021Y0065);福州大学科研启动项目(XRC-22038,XRC-22039);福州大学开放测试基金 (2022T030,2022T031);基本科研业务费专项资金(2017028)


Structure and Properties of Biodegradable Poly(butylene adipateterephthalate)/ Polylactic Acid Packaging Films with Isophorone Diisocyanate as Reactive Compatibilizer
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    以异佛尔酮二异氰酸酯(IPDI)为聚己二酸-对苯二甲酸丁二酯/聚乳酸(PBAT/PLA)共混物的增容剂,通过熔融共混法制备了PBAT/PLA/IPDI共混粒子并吹制得到薄膜。采用红外光谱、扫描电镜、差示扫描量热分析、拉伸试验、热重分析和水蒸气透过率测试等研究了不同含量IPDI对共混薄膜形态结构、结晶性能、力学性能、热性能和阻隔性能的影响。结果表明,IPDI的异氰酸酯基团能与PBAT和PLA发生化学反应,分散相尺寸变小,两相界面变得模糊,有效改善了共混物的相容性。随着IPDI含量的增加,共混物中PBAT的结晶度升高,薄膜的拉伸强度逐渐增大,水蒸气阻隔性能呈现先增大后减小的趋势。当IPDI质量分数为0.5%时,PBAT/PLA/IPDI薄膜的横纵向拉伸强度相较于纯PBAT/PLA薄膜分别提升了74.2%和28.6%,断裂伸长率维持在790%和244%,水蒸气透过率降低了38.2%,表现出良好的力学和水蒸气阻隔等综合性能。

    Abstract:

    Isophorone diisocyanate (IPDI) as reactive compatibilizer was introduced into poly(butylene adipateterephthalate) (PBAT)/polylactic acid (PLA) blend by melt blending and extruded into blown films. The effect of IPDI content on the phase morphology, crystallization behavior, mechanical, thermal and barrier properties of PBAT/PLA/IPDI blended films were investigated by Fourier transform infrared spectroscopy (FT-IR), scanning electron microscope(SEM), differential scanning calorimeter (DSC), universal tensile testing machine, thermogravimetric analyzer (TGA) and water permeability tester. Results demonstrate that the —NCO groups of IPDI can chemically react with PBAT and PLA to form copolymer, which reduces the particle size of PLA dispersed phase and leads to indistinct interface between the two-phase, effectively improving the interfacial compatibility between PBAT and PLA matrix. With increasing the IPDI content in PBAT/PLA/IPDI films, the crystallization ability of PBAT matrix and tensile strength increase, whilst the water vapor barrier performance increases first and then decreases. When the mass fraction of IPDI is 0.5% , compared with the pristine PBAT/PLA film, the PBAT/PLA/IPDI packaging film shows 74.2% and 28.6% enhancement in tensile strength on the transverse direction and machine direction, respectively, maintains decent breaking elongation of 790% and 244%, meanwhile, 38.2% reduction in water vapor permeability coefficient, which suggests the balanced overall mechanical and water vapor barrier properties.

    参考文献
    相似文献
    引证文献
引用本文

毛 帅,龚佳荣,孙文涛,宁博远,罗耀发,许平凡, 刘源森,蓝小平,章培昆,刘 渊.异佛尔酮二异氰酸酯反应增容聚己二酸-对苯二甲酸丁二酯/聚乳酸生物降解阻隔膜的结构与性能[J].高分子材料科学与工程,2023,39(8):148-155. Shuai Mao, Jiarong Gong, Wentao Sun, Boyuan Ning, Yaofa Luo, Pingfan Xu, Yuansen Liu, Xiaoping Lan, Peikun Zhang, Yuan Liu. Structure and Properties of Biodegradable Poly(butylene adipateterephthalate)/ Polylactic Acid Packaging Films with Isophorone Diisocyanate as Reactive Compatibilizer[J]. Polymer Materials Science & Engineering,2023,39(8):148-155.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2023-10-11
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有