Abstract:Phenolic (PR) aerogel has outstanding advantages such as low density and low thermal conductivity, which is widely used as thermal insulation material. The traditional preparation processes of PR aerogel are complex, and PR aerogel is inherently hygroscopic. In this study, silicon- modified phenolic resins were prepared by chemical grafting and physical blending using linear phenolic resin as raw material and octyltriethoxysilane (OTES) as hydrophobic modifier, and then silicon-modified phenolic aerogels were prepared by sol-gel and atmospheric pressure drying process. The aerogels were characterized by scanning electron microscopy and energy spectroscopy, N2 adsorption-desorption experiment, synchronous thermal analysis, thermal constant and hydrophobic angle measurement, and the water absorption performance was evaluated by water immersion experiment. The density of the prepared samples is between 0.205~0.260 g/cm3, and the thermal conductivities are 0.040~0.044 W/(m·K). The results show that OTES improves the thermal stability, hydrophobicity and thermal insulation performance of PR aerogels, and the comprehensive performance of chemical grafting method is better than that of physical blending method. The physical blending modification increases the high temperature residual mass rate of aerogels by about 5%, the hydrophobic angle is increased by 129°, and the saturated moisture absorption rate in water is 59.6% (up to 349.5% before modification). The addition of a small amount of OTES through the chemical grafting route can greatly improve the performance of aerogels, the residual mass rate is increased by about 10%, the hydrophobic angle is 153.4°, and the saturation moisture absorption rate is only 19.6%.