氧化石墨烯改性玄武岩纤维/聚酰亚胺复合材料的制备与摩擦学性能
作者:
作者单位:

作者简介:

通讯作者:

中图分类号:

基金项目:

四川省科技计划项目(2023YFG0239);四川轻化工大学科研创新团队计划项目(H92322);机械结构优化及材料应用泸州市重点实验室开放课题(SCHYZSB-2023-01, SCHYZSA-2023-01);2023年四川轻化工大学大学生创新创业项目(CX2023072)


Preparation and Tribological Performance of Graphene Oxide Modified Basalt Fiber/Polyimide Composites
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    通过静电自组装法将氧化石墨烯(GO)附着在硅烷偶联剂KH550接枝后的玄武岩纤维表面,并采用热模压工艺制备了GO 改性玄武岩纤维/聚酰亚胺复合材料(GBF/PI)。对比研究了聚酰亚胺(PI)、玄武岩纤维/聚酰亚胺(BF/PI)、KH550改性玄武岩纤维/聚酰亚胺(KBF/PI)、GBF/PI复合材料的力学性能和摩擦磨损性能。结果表明,GBF/PI复合材料的维氏硬度、压缩强度和弯曲强度分别为66.5 HV,275.9 MPa和169.8 MPa,较PI试样分别提高约29.2%,45.8%和47.1%,较BF/PI试样分别提高约21.9%,27.0%和28.1%,较KBF/PI试样分别提高约6.9%,20.2%和10.2%。与PI,BF/PI和 KBF/PI 试样相比,GBF/PI 复合材料具有更优的热稳定性,其中 GBF/PI 的起始分解温度和质量残留率分别为398.4 ℃和57.70%,明显高于PI树脂的387.5 ℃和49.36%。摩擦磨损实验结果表明,与GCr15对磨60 min后,GBF/PI的平均摩擦系数为0.617,磨损率为5.22×10?6 mm3/(N·m),较PI树脂试样分别低约11.4%和47.2%,较BF/PI试样分别低约7.7%和27.0%,较KBF/PI试样分别低约8.4%和12.0%。GO的引入有利于形成致密均匀的摩擦层,减轻了PI基复合材料摩擦损伤,提高了材料的减磨抗磨性能。

    Abstract:

    By electrostatic self- assembly method, graphene oxide (GO) was adhered to the surface of basalt fibers grafted with silane coupling agent KH550, followed by the fabrication of GO- modified basalt fiber/polyimide composite material (GBF/PI) by hot compression molding process. The mechanical and frictional-wear properties of polyimide (PI), basalt fiber/polyimide (BF/PI), KH550- modified basalt fiber/polyimide (KBF/PI), and GBF/PI composite materials were comparative investigated. The results indicate that the Vickers hardness, compressive strength, and flexural strength of the GBF/PI composite are 66.5 HV, 275.9 MPa, and 169.8 MPa, respectively. These values reveal enhancements of approximately 29.2%, 45.8%, and 47.1% compared to the PI specimens, 21.9%, 27.0% and 28.1% compared to the BF/PI specimens, and 6.9%, 20.2% and 10.2% compared to the KBF/PI specimens, respectively. In comparison with the PI, BF/PI and KBF/PI specimens, the GBF/PI composites have superior thermal stability, in which the onset decomposition temperature and mass residual rate of GBF/PI are 398.4 ℃ and 57.70% , respectively, which are significantly higher than those of the PI resins at 387.5 ℃ and 49.36%. Frictional-wear test results indicate that after 60 min of sliding against GCr15, the average friction coefficient of GBF/PI is 0.617, and the wear rate is 5.22×10?6 mm3/(N·m). These values are approximately 11.4% and 47.2% lower than those of the PI specimens, 7.7% and 27.0% lower than the BF/PI specimens, and 8.4% and 12.0% lower than the KBF/PI specimens. The introduction of GO facilitated the formation of dense and uniform friction layer, mitigating frictional damage to the PI- based composites and enhancing their anti- wear performance.

    参考文献
    相似文献
    引证文献
引用本文

李 轩,周德东,何 瑜,张立京,吕 威,张续译,杨远鹏,刘志章.氧化石墨烯改性玄武岩纤维/聚酰亚胺复合材料的制备与摩擦学性能[J].高分子材料科学与工程,2024,40(5):76-86. Xuan Li, Dedong Zhou, Yu He, Lijing Zhang, Wei Lü, Xuyi Zhang, YuanpengYang, Zhizhang Liu. Preparation and Tribological Performance of Graphene Oxide Modified Basalt Fiber/Polyimide Composites[J]. Polymer Materials Science & Engineering,2024,40(5):76-86.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2024-07-17
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司