Abstract:In this study, natural latex (NRL)/styrene-butadiene latex (SBRL) water latex paste was prepared by replacing the traditional oily rubber paste preparation method with green and environmentally friendly water latex slurry, and the viscosity of the slurry, vulcanization characteristics of the blended rubber after drying, mechanical properties at room temperature and high temperature and wear resistance were determined. At the same time, NR/SBR/polyester cotton composites were prepared with glue, the peeling strength of the composites was determined, and the influence of SBR dosage on the properties of the composites was studied by combination with bulk microscopy, SEM and other characterization methods. The results show that in terms of slurry, with the increase of SBRL dosage, the viscosity of the slurry first increases and then decreases. The positive vulcanization time (t90) of the blended rubber is gradually extended, the maximum torque (MH) of vulcanization curve is increased, the constant tensile stress at room temperature and high temperature (60 ℃) is increased, and the wear resistance is effectively improved. In terms of adhesive adhesion, the peeling strength gradually decreases with the increase of SBRL dosage. Bulk microscopy and SEM show that with the increase of SBRL ratio, the amount of adhesive attached to the surface of fiber cloth after peeling of the specimens gradually decreases, and the reason for the decline in peeling strength is reflected in the side.