Abstract:Preparing high-concentration polyimide (PI) solutions via the dissolution method is an effective approach to enhance both production efficiency and product performance in PI fiber manufacturing. However, increasing PI concentration often leads to reduced solution homogeneity and stability. To address this challenge, this study used a ternary copolymer of benzophenone tetracarboxylic dianhydride with toluene diisocyanate and diphenylmethane-4,4'-diisocyanate as the raw material, and selected two commonly used PI solvents N-methylpyrrolidone (NMP) and N,N-dimethylacetamide (DMAc) to prepare PI solutions with mass fractions ranging from 15 wt% to 32 wt%. The intrinsic relationship between solution concentration and its homogeneity and stability was investigated through rheological analysis. Results show that NMP, due to its rigid cyclic molecular structure and excellent solvating ability, effectively suppresses PI chain folding and phase separation, making it suitable for preparing high-concentration PI solutions. The critical entanglement concentration of PI/NMP solutions is approximately 27 wt%; at this concentration, the onset shear rate of shear thinning during steady-state shear scanning significantly decreases, while zero-shear viscosity and relaxation time increase, indicating pronounced shear-thinning behavior and viscoelastic response. When the concentration increases to 32 wt%, the overlap between steady-state apparent viscosity and dynamic complex viscosity in the low-frequency region diminishes, revealing heterogeneous characteristics and greater sensitivity to temperature changes. Therefore, considering the homogeneity and stability of PI solutions, NMP is recommended as the preferred solvent, with solution concentration ideally maintained between 27 wt% and 30 wt%.