Abstract:To overcome the inherent hydrophilicity of polyimide (PI) aerogels and improve their cyclic oil-water separation performance, a PI/polybenzoxazine/polyhexahydrotriazine (PI/PBOZ/PHT) composite aerogel was constructed by room-temperature aldehyde-amine cross-linking followed by stepwise thermal curing. FT-IR spectra show characteristic imide C=O bands at 1772 cm-1and 1721 cm-1, and imide C–N bands at 1357 cm-1 and 732 cm-1; PHT-related C–N bands appear at 1114 cm-1 and 790 cm-1, while the Si–O–Si asymmetric stretching band is observed at 1056 cm-1, confirming formation of the composite network. SEM reveals a 3~15 μm interconnected porous structure in which PBOZ/PHT connects the PI framework. The water contact angle increases from 102° for PI to 122° for PI/PBOZ/PHT. Adsorption capacities for various oils and organic solvents reach 36~60 g/g, and 95.1% of the adsorption capacity is retained after 10 dichloromethane adsorption-desorption cycles. The combined effects of low-surface-energy groups and a cross-linked porous network account for the improved hydrophobicity and cycling stability.