热塑性聚酰胺弹性体改性乙烯-醋酸乙烯共聚物 及其发泡行为
DOI:
作者:
作者单位:

常州大学 材料科学与工程学院,江苏 常州 213164

作者简介:

通讯作者:

中图分类号:

基金项目:

江苏省研究生科研与实践创新计划项目(KYCX223030)


Modification of PEBAX with EVA and Its Foaming Behavior
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    乙烯-醋酸乙烯共聚物(EVA)发泡材料存在耐温性能差、力学与回弹性能不足等问题,将热塑性弹性体与乙烯-醋酸乙烯共聚物共混改性是获得高性价比EVA发泡材料的有效途径。本文选用新型热塑性聚酰胺弹性体(PEBAX)与EVA共混,采用马来酸酐接枝乙烯-醋酸乙烯酯(EVA-g-MAH)为增容剂,通过熔融共混制备EVA/PEBAX共混物,然后再化学发泡制备EVA发泡材料,考察相容化前后及发泡对相关材料性能的影响。结果表明:随着PEBAX含量的提升,EVA/PEBAX简单共混物拉伸强度和断裂伸长率下降,定伸强度提高,拉伸永久变形下降;对于EVA/PEBAX增容共混物,随着EVA-g-MAH用量增加,共混物(EVA/PEBAX(质量比70/30))力学性能明显提高,当EVA-g-MAH含量为20%时,共混物性能已经明显高于纯EVA性能,EVA-g-MAH能够有效增容EVA/PEBAX共混物;SEM显示:增容后,两相界面模糊,分散相尺寸明显减小。共混物发泡材料性能测试表明:随着EVA-g-MAH用量增加,其拉伸强度、断裂伸长率、撕裂强度、回弹率明显提高,且呈现先升高后降低的趋势;泡孔尺寸变小,分布变窄;与纯EVA发泡材料热收缩率11%左右相比,共混物的热收缩率为2.65%左右,明显降低。当EVA-g-MAH含量为20%时,EVA/PEBAX(质量比70/30)发泡材料综合性能最佳。

    Abstract:

    Ethylene-vinyl acetate (EVA) foamed materials suffer from poor heat resistance and insufficient mechanical and rebound properties. Blending thermoplastic elastomers with EVA is an effective approach to obtain high-performance, cost-effective EVA foam materials. In this study, a novel thermoplastic polyamide elastomer (PEBAX) was blended with EVA, using maleic anhydride grafted ethylene-vinyl acetate (EVA-g-MAH) as a compatibilizer. The EVA/PEBAX blend was prepared via melt mixing, followed by chemical foaming to produce the EVA foam material. The effects of compatibilization and foaming on the material properties were investigated. Results show that as PEBAX content increases, the tensile strength and elongation at break of the simple EVA/PEBAX blend decrease, while the stress at 100% elongation increases and permanent set decreases. For the compatibilized EVA/PEBAX blend, increasing the amount of EVA-g-MAH significantly improves mechanical properties. When the EVA-g-MAH content reaches 20%, the blend performance surpasses that of pure EVA, indicating that EVA-g-MAH effectively enhances compatibility in the EVA/PEBAX system. SEM analysis reveals that after compatibilization, the interface between the two phases becomes blurred and the dispersed phase size is significantly reduced. Performance tests of the foamed blends indicate that with increasing EVA-g-MAH content, tensile strength, elongation at break, tear strength, and rebound rate all improve markedly, showing a trend of initial increase followed by decline. Cell size decreases and distribution becomes narrower. Compared to pure EVA foam materials, which exhibit a thermal shrinkage of about 11%, the thermal shrinkage of the blend is only around 2.65%, representing a significant reduction. When the EVA-g-MAH content is 20%, the EVA/PEBAX (70/30 wt%) foam material achieves optimal overall performance.

    参考文献
    相似文献
    引证文献
引用本文
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2025-10-30
  • 录用日期:2026-09-16
  • 网络出版日期:2026-10-16
  • 在线发布日期:
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司