Abstract:In this study, a series of poly(ethylene 2, 5- furandicarboxylate- co- ethylene terephthalate) copolyesters (PEFT) with different dimethyl 2, 5- furandicarboxylic acid (DMFD) monomer contents were prepared from biobased monomer DMFD by copolymerization with dimethyl terephthalate (DMT) and ethylene glycol (EG) by ester- exchange melt polycondensation. The absolute molecular weight and molecular weight distribution of the copolyesters by APC-MALLS-RID. By 1H-NMR, FT-IR, DSC, TGA, XRD and other testing methods, the effects of DMFD monomer content on the polymerization reaction kinetics, chemical structure, molecular weight and molecular weight distribution, thermal properties, crystallinity and mechanical property of the PEFT co-polyesters were investigated. The results show that the PEFT copolyester was successfully prepared in accordance with the molecular weight requirement of fiber grade; the reaction kinetics study shows that the transesterification reaction was mainly concentrated at the early stage of the reaction (0~35 min), which is in line with the characteristics of the gradual polymerization mechanism in polyester polycondensation reaction; with the increase of DMFD monomer content, the glass transition temperature (Tg) of PEFT copolyester increases linearly, and the thermal decomposition temperature decreases, tensile strength and elongation at break first increase and then decrease. When the content of DMFD monomer exceeds 20%, the copolyester could not be crystallized because the regularity is destroyed.