Abstract:Poly (4-hydroxybutyrate) (P4HB) is a biodegradable aliphatic polyester with advantages such as high toughness, excellent degradation rate, and good biocompatibility of degradation products. However, its processing and application are limited by its low melt strength and crystallization rate. In order to improve the melt strength and crystallization rate of P4HB, aromatic 4, 4'- diphenylmethane diisocyanate (MDI) and aliphatic hexamethylene diisocyanate (HDI) were selected as chain extenders. P4HB was chain extended via melt reaction by the catalysis of dibutyltin dilaurate (DBTDL). The amount of catalyst and chain extenders was optimized. The effects of isocyanates chain extender on the melt strength, crystallization behavior, and mechanical properties of poly (4-hydroxybutyrate) was systematically studied. Research has found that MDI can better enhance the melt strength and mechanical properties of P4HB, while HDI can better increase the crystallization temperature and rate of P4HB. When the mole ratio of P4HB to MDI is 1:3, the impact strength of P4HB increases from 8.4 kJ/m2 to 25.1 kJ/m2, and the melt flow rate decreases from 158 g/10 min to 20 g/10 min. When the mole ratio of P4HB to HDI is 1:2.5, the crystallization temperature of P4HB increases from 20.8 ℃ to 32.6 ℃.