Abstract:As artificial grass silk carpets, polyethylene extruded and stretched filament is comfortable, soft and elastic, but its performance still has the problem of conflict between high resilience and low shrinkage. In this article, the relationship between the structure and properties of pre- stretched linear low density polyethylene/ bimodal linear low density polyethylene/polyolefin elastomer (LLDPE/BLLDPE/POE) blends were investigated. When the pre-stretched ratio λ=5, the tensile strength of LLDPE/BLLDPE/POEλ5 increases from 43.6 MPa to 81.9 MPa, and the length of critical defects increases from 4.2 mm to 9.9 mm, which has good mechanical properties. The resilience experiment and shrinkage experiment show that compared with LLDPE/POEλ5, the final deformation recovery of LLDPE/BLLDPE/POEλ5 increases from 69% to 84% at 50 ℃, and the shrinkage of 100 min at 80 ℃ decreases from 9.4% to 5.5%, with a high resilience and low shrinkage. The melt tensile test results show that the melt tensile stress of LLDPE/BLLDPE/POE reaches 410 kPa, and the melt stretch ratio reaches 10.3, showing good processability. The results of this study provide an effective method for the development of highperformance modified PE rayon filaments.