    摘要:

    文中采用4种不同厚度的复合材料补片,对含10 mm裂纹损伤的碳纤维增强热固性复合材料(CFRP)开展了超声修复试验,在待修复试样与补片之间预置热塑薄膜,薄膜为0.2 mm厚的聚醚醚酮(PEEK)树脂。结果显示,补片厚度对修复试样的力学性能和失效形式具有显著影响。随着补片厚度增加,修复试样的力学性能呈先增大后减小的趋势,较厚补片会降低修复试样的力学性能及成型效果。其中,补片厚度为2.627 mm时,拉伸强度最高可达392.7 MPa,强度恢复率可达77.8%;补片厚度为2.660 mm时,试验件的极限承载能力下降了1200.2 N,拉伸强度降为370.5 MPa,修复试样变形量最大,高达0.056 mm。通过扫描电镜对修复试样的失效形式进行分析,发现失效机制随补片厚度变化而不同,对于补片厚度为0.627 mm的试验件,失效模式主要为混合失效。

    Abstract:

    Four different thicknesses of composite patches were used to conduct ultrasonic repair experiments on carbon fiber-reinforced thermosetting composites (CFRP) with 10 mm crack damage. A thermoplastic thin film was placed between the repaired sample and the patch, with a thickness of 0.2 mm of polyether ether ketone (PEEK) resin. The results show that the thickness of the patch has a significant impact on the mechanical properties and failure modes of the repaired specimens. As the thickness of the patch increases, the mechanical properties of the repaired specimens show a trend of first increasing and then decreasing. Thicker patches will reduce the mechanical properties and forming effect of the repaired specimens. Among them, when the thickness of the patch is 2.627 mm, the maximum tensile strength can reach 392.7 MPa, and the strength recovery rate can reach 77.8%; when the thickness of the patch is 2.660 mm, the ultimate bearing capacity of the test piece is decreased by 1200.2 N, the tensile strength decreases to 370.5 MPa, and the maximum deformation of the repaired sample is as high as 0.056 mm. Through scanning electron microscopy analysis of the failure mode of the repaired specimens, it is found that the failure mechanism varies with the thickness of the patch. For the test piece with a patch thickness of 0.627 mm, the main failure mode is interface fracture.

    参考文献
    相似文献
    引证文献
引用本文

肖 丽,高奇玉,卜珩倡,朱洪伟,李斌斌,占小红.基于预置热塑薄膜的碳纤维增强热固性复合材料含裂纹损伤层合板超声修复的拉伸性能[J].高分子材料科学与工程,2025,41(6):77-87. Li Xiao, Qiyu Gao, Hengchang Bu, Hongwei Zhu, Binbin Li, Xiaohong Zhan. Tensile Performance of Ultrasonic Repair of Carbon Fiber-Reinforced Thermosetting Composites Laminates with Crack Damage Based on Pre-Set Thermoplastic Films[J]. Polymer Materials Science & Engineering,2025,41(6):77-87.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2025-09-24
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司