Abstract:Currently, the synthesis of bicyclopentadiene- phenol epoxy resin monomers (EMR- EP) mainly involves improving the catalytic efficiency by adding phase transfer catalysts and co- solvents, which leads to issues such as a high number of byproducts, difficulty in separating the products, and higher chlorine content. In response to these problems, a synthesis process without phase transfer catalysts and using low-boiling, low-toxicity co- solvents was proposed. During the ring- opening stage, the epoxy equivalent increases with the addition of sodium hydroxide (NaOH), reaching 276 g/eq when the NaOH content is 0.5%of the total raw material amount. In the ring- closing stage, the epoxy equivalent decreases with the addition of NaOH, reaching 275 g/eq when the NaOH content is 1.8 times the amount of phenolic hydroxyl groups. In the purification process, a method of first removing inorganic salts and then dechlorinating was adopted to solve the problem of excessively high hydrolytic chlorine content. In the refining process, using a 49%NaOH aqueous solution with the addition amount of 25% of the total mass of phenol, the hydrolytic chlorine content of the monomer is stabilized within 0.02%, and the total chlorine content is significantly reduced. The infrared test results confirm the successful introduction of epoxy groups, and GPC analysis show that the dibicyclopentadiene- phenol resin synthesized in this study and the commercially produced foreign BSE095 have the maximum peak at the same retention time, indicating the successful synthesis of electronic grade bicyclopentadiene-phenol epoxy resin monomers.