    摘要:

    以六氯环三磷腈(HCCP)和4,4'-二羟基二苯砜(BPS)为原料,通过亲核取代合成了聚磷腈(Poly(HCCP-co-BPS),PHB)微球。 将3-氨丙基三乙氧基硅烷(APTES)和蒙脱土(Na-MMT)进行反应,制备了硅烷偶联剂改性蒙脱土(AP-MMT)。 以四甲基间苯二亚甲基二异氰酸酯(TMXDI)为单体,在催化剂作用下,经缩聚反应合成了抗水解剂聚碳化二亚胺(PCDI)。 将PHB和AP-MMT作为阻燃剂,PCDI作为抗水解剂,加入到PET基材中,经过熔融共混制备了PET/PHB/AP-MMT/PCDI 阻燃耐水解复合材料,研究了复合材料的阻燃性能和耐水解性能。 结果表明,随着PHB 和AP-MMT添加量的增加,两者发挥了协同阻燃作用,复合材料阻燃性能明显增强;添加PCDI后,由于其消耗了聚酯体系中的羧基,并与羟基反应促使材料局部交联,材料抗水解性能及力学性能显著提升。 当配方组成为PET/1.5%PHB/2.0%AP-MMT/1.0%PCDI 时,LOI 值达到27.3%,阻燃等级为 V-0,且在水解老化 96 h 后,拉伸强度保持率达到85%,端羧基含量明显下降。

    Abstract:

    Poly (HCCP-co-BPS) microspheres were synthesized by nucleophilic substitution using phosphonitrilic chloride trimer (HCCP) and 4,4′-dihydroxydiphenyl sulfone(BPS) as raw materials. Using 3-aminopropyltriethoxysilane (APTES) as modifier and montmorillonite (Na-MMT) as raw material, silane coupling agent modified montmorillonite (AP-MMT) was obtained. Starting from tetramethyl isophthalic diisocyanate (TMXDI), under catalytic conditions, the hydrolysis resistant agent carbodiimide (hereinafter referred to as PCDI) was obtained. Using PHB and AP-MMT as flame retardants, and PCDI as anti hydrolysis agent to PET substrate, PET/PHB/AP-MMT/PCDI flame retardant and hydrolysis resistant composite materials were prepared by melt blending, and the flame retardant and hydrolysis resistant properties of the composite materials were studied. The results show that with the increase of PHB and AP-MMT addition, the flame retardancy of the composite materials is significantly enhanced; after adding PCDI, carboxyl groups in the polyester system are consumed, and the reaction with hydroxyl groups promotes local cross-linking of the material, which significantly improves the hydrolysis resistance and mechanical properties of the material. When the formula is composed of PET/1.5% PHB/2.0% AP-MMT/1.0% PCDI, the limiting oxygen index (LOI) reaches 27.3%, the flame retardant grade is V-0, and the tensile strength retention rate reaches 85% after 96 h of hydrolysis aging, and the content of terminal carboxyl group decreases significantly.

    参考文献
    相似文献
    引证文献
引用本文

陶家骏, 徐梦楠, 佴 妍, 苏成龙, 蒋 姗. PET/PHB/AP-MMT/PCDI 阻燃耐水解复合材料制备及性能[J].高分子材料科学与工程,2025,41(10):1-12. Jiajun Tao, Mengnan Xu, Yan Nai, Chenglong Su, Shan Jiang. Preparation and Performance of PET/PHB /AP-MMT/PCDI Flame Retardant and Hydrolytic Resistant Composite Materials[J]. Polymer Materials Science & Engineering,2025,41(10):1-12.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2026-03-17
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司