六钛酸钾晶须对玄武岩纤维/聚酰亚胺复合材料摩擦磨损性能的影响
作者:
作者单位:

作者简介:

通讯作者:

中图分类号:

基金项目:

四川省科技计划项目(2023YFG0239); 宜宾市科技计划重点研发项目(2024GY001); 四川轻化工大学科研创新团队计划项目(H92322); 泸州市智能机电控制工程技术研究中心开放课题(ZNJDKT25-01); 四川轻化工大学研究生基金项目(Y2024016); 2024 年四川轻化工大学大学生创新创业项目(CX2023072)


Effect of Potassium Titanate Whiskers on the Friction and Wear Performance of Basalt Fiber/Polyimide Composites
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    采用热模压方法制备了六钛酸钾晶须(PTW)和氧化石墨烯改性玄武岩纤维(GBF)混杂改性的聚酰亚胺复合材料(PTW-GBF/PI),研究了PTW 含量对复合材料显微结构、力学性能、耐热性能和摩擦磨损性能的影响。随PTW 含量增加,复合材料的硬度上升,压缩强度和弯曲强度呈先增加后降低的趋势;其中,PTW 质量分数为6% 时,PTWGBF/PI 复合材料的压缩强度和弯曲强度均达到最大值,分别为236.62 MPa 和217.34 MPa,较GBF/PI 复合材料分别提高约14.8% 和36.6% ,表明PTW 质量分数在6% 时实现了最佳的协同增强效果,其在基体中的桥联、应力传递有效提升了界面结合与能量耗散能力,与GBF 起到了良好的协同增强效果。摩擦磨损实验结果表明,适量PTW 的引入显著改善了复合材料的摩擦性能,当PTW 质量分数为6% 时,复合材料在5 N,10 和15 N 载荷下均具有最低的平均摩擦系数(0.506,0.323 和0.291)和磨损率(6.75×10-6 mm3/( N·m), 6.04×10-6 mm3/( N·m) 和4.82×10-6 mm3/( N·m))。GBF/PI 和PTW-GBF/PI 复合材料的磨损均以疲劳磨损和犁削磨损为主,伴随有黏着磨损和磨粒磨损;适量添加PTW(6% )对疲劳磨损、犁削磨损和黏着磨损具有显著抑制作用,但质量分数过高(9% ) 会因晶须团聚导致疲劳磨损加剧。

    Abstract:

    The potassium titanate whisker (PTW) and graphene oxide-modified basalt fibers (GBF)hybridmodified polyimide composites (PTW-GBF/PI) were prepared through hot pressing method. The effects of PTW content on the mechanical properties, thermal stability, and friction-wear performance of the composites were investigated. As the PTW content increases, the hardness of the composites increases, while the compressive strength and flexural strength initially increase and then decrease. When the PTW mass fraction is 6% , the compressive strength and flexural strength of PTW-GBF/PI composite show the maximum values of 236.62 MPa and 217.34 MPa, respectively, which are approximately 14.8% and 36.6% higher than those of GBF/PI composite. The above observation indicates that when the PTW mass fraction is 6% , the composite achieves the optimal synergistic reinforcement effect. The bridging and stress-transfer functions of PTW within the matrix effectively enhance the interfacial bonding and energy dissipation capability, exhibiting excellent cooperative strengthening behavior with GBF. The results of friction-wear tests indicate that the introduction of appropriate amount of PTW significantly improve the tribological performance of composite. When the PTW mass fraction is 6% , the composite exhibits the lowest average coefficient of friction (0.506, 0.323, and 0.291) and wear rate (6. 75×10-6 mm3/( N·m), 6.04×10-6 mm3/( N·m), and 4.82×10-6 mm3/( N·m)) under loads of 5 N, 10 N, and 15 N, respectively. The wear of GBF/PI and PTW-GBF/PI composites is primarily characterized by fatigue wear and plowing wear, accompanied by adhesive wear and abrasive wear. The appropriate PTW addition (mass fraction of 6% ) significantly inhibits fatigue wear, plowing wear, and adhesive wear; however, excessive PTW content (9% ) leads to increased fatigue wear due to whisker agglomeration.

    参考文献
    相似文献
    引证文献
引用本文

刘 明, 李 轩, 周德东, 蒋 杰, 王朝健, 杨远鹏, 邓 瑞, 林小薇, 刘志章, 张续译.六钛酸钾晶须对玄武岩纤维/聚酰亚胺复合材料摩擦磨损性能的影响[J].高分子材料科学与工程,2025,41(12):95-105. Ming Liu, Xuan Li, Dedong Zhou, Jie Jiang, Chaojian Wang, Yuanpeng Yang, Rui Deng, Xiaowei Lin, Zhizhang Liu, Xuyi Zhang. Effect of Potassium Titanate Whiskers on the Friction and Wear Performance of Basalt Fiber/Polyimide Composites[J]. Polymer Materials Science & Engineering,2025,41(12):95-105.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2026-03-21
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司