Abstract:To address the complex fabrication process and high energy consumption of polyamide elastomers, together with the weak interlayer bonding and high porosity of high-speed-sintered (HSS) parts, a high-performance dynamic poly(urea-amide) (PUA) elastomer was designed, with its performance regulated by acylsemicarbazide (ASC) dynamic bonds formed in the hard segments. Rheological analysis, dynamic mechanical analysis (DMA), and hot-stage microscopy revealed the sintering window and melting behavior of the PUA elastomer. After optimization of the printing parameters, parts with good mechanical performance and dimensional accuracy were obtained at a scanning speed of 24 mm s?1 and a layer thickness of 0.2 mm. Thermal annealing and vacuum-assisted infiltration were further applied as post-treatment strategies: the thermally activated dynamic bonds promoted interlayer healing, while the low-viscosity infiltrating liquid filled the internal pores. Consequently, the tensile strength increased from 1.06 MPa to 18.12 MPa, and the elongation at break increased from 72.4% to 316.2%, with markedly reduced porosity and significantly improved surface morphology. This work provides a new strategy for the fabrication of high-performance, repairable, and recyclable 3D-printed parts.