    摘要:

    研究了聚合体系 pH 和共聚单体投料比对丙烯腈( AN)-甲基丙烯磺( SMAS)共聚物结构和性能的影响。 结果表明,在相同聚合条件下,AN-SMAS 共聚物转化率、相对分子质量和黏度远小于均聚物;聚合体系的 pH 值由 7.2 降低到 2,AN 反应性增加,共聚物亲水性降低;共聚物的转化率由 82.9% 增加到 88.2% ,重均分子量由 20120 增加到25430,黏度由 7.08 Pa·s 增加到 62.7 Pa·s,接触角由 32.9°增加到 43.0°。 增加 SMAS 单体的投料比,AN 反应性减小,共聚物中磺酸基团的比例增加,共聚物的亲水性提高。 综合考虑共聚物可纺性和亲水性,控制聚合体系 pH 为 3.5,SMAS 投料比为 3.3% ,得到黏度为 18.4 Pa·s,接触角为 34.6°的共聚物。 湿法纺丝制得外直径为 535.3 μm,内直径为409.6 μm,中空度为 58.5% ,含水率达 59.5% 的中空纤维。

    Abstract:

    The effects of polymerization pH system and comonomer ratio on the structure, conversion, relative molecular weight, viscosity and hydrophilicity of acrylonitrile ( AN)-sodium methacrylate sulfonate ( SMAS) copolymer were studied by Fourier infrared spectroscopy ( IR), nuclear magnetic resonance ( NMR), gel permeation chromatography (GPC), rotary rheometer, contact angle test, etc. The results show that under the same polymerization conditions, the conversion rate, relative molecular weight and viscosity of AN-SMAS copolymers are much lower than those of homopolymers; lowering pH value of the polymerization system increases the reactivity of AN and decreases the hydrophilicity of the copolymer. At pH = 2, the conversion rate of the copolymer increases from 82.9% to 88.2% , the weight average molecular weight increases from 20120 to 25430, the viscosity increases from 7.08 Pa·s to 62.7 Pa·s, and the contact angle increases from 32.9° to 43.0°. Increasing the feeding ratio of SMAS monomer reduces the reactivity of AN, the proportion of sulfonic acid groups in the copolymer increases, and the hydrophilicity of the copolymer is improved. Taking into account the spinnability and hydrophilicity of the copolymer, pH of the polymerization system is controlled at 3.5, and the SMAS feeding ratio is 3.3% , resulting in a copolymer with a viscosity of 18.4 Pa·s and a contact angle of 34.6°. Hollow fibers with an outer diameter of 535.3 μm, an inner diameter of 409.6 μm, a hollow degree of 58.5% , and a moisture content of 59.5% were produced by wet spinning.

    参考文献
    相似文献
    引证文献
引用本文

刘宇涛, 柳 雷, 曹钰婷, 朱慧萱, 李常清.亲水性丙烯腈/甲基丙烯磺酸钠共聚物制备及其结构[J].高分子材料科学与工程,2026,42(2):19-27. Yutao Liu, Lei Liu, Yuting Cao, Huixuan Zhu, Changqing Li. Preparation and Structure of Hydrophilic Acrylonitrile/Sodium Methacrylate Sulfonate Copolymer[J]. Polymer Materials Science & Engineering,2026,42(2):19-27.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2026-05-10
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司