嵌段聚合物 PBAT-b-PLA 在共混物 PBAT/PBAT-b-PLA/PLA中的增容作用及对共混物性能的影响
作者:
作者单位:

作者简介:

通讯作者:

中图分类号:

基金项目:

国家自然科学基金资助项目(52173104);四川省自然科学基金资助项目( 2024NSFSC1031);天府永兴实验室研究项目基金(2023KJGG12)


Compatibilizing Effect of Block Polymer PBAT-b-PLA in PBAT/ PBAT-b-PLA / PLA Blends and Its Influence on Blend Properties
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为开发兼具聚对苯二甲酸-己二酸丁二醇酯(PBAT)和聚乳酸(PLA)性能优势的共混物新材料,文中将嵌段聚合物 PBAT-b-PLA 引入到 PBAT 与 PLA 的共混体系中得到三元共混物 PBAT/ PBAT-b-PLA/ PLA,系统研究了嵌段聚合物在共混物中的增容作用和对共混物力学性能、光学性能和气体阻隔性能的影响。 差示扫描量热分析和扫描电子显微镜结果表明,PBAT-b-PLA 能显著提升 PBAT 与 PLA 之间的相容性,分散相尺寸和两相玻璃化转变温度差值(ΔTg)分别由 PBAT/ PLA 体系的 5712 nm 和 94.22 ℃降至 1200 nm 和 94.00 ℃以下;分散相尺寸随嵌段聚合物数均分子量降低而减小,PBAT-b-PLA 数均分子量从 8.5×104 减小到 3.0×104,分散相尺寸由 1186 nm 降至 426 nm。 PBAT-bPLA 的增容作用使 PBAT/ PBAT-b-PLA/ PLA 的性能优于 PBAT/ PLA,并随 PBAT-b-PLA 的数均分子量变化而变化。随着 PBAT-b-PLA 数均分子量由 8.5×104 减小到 3.0×104,三元共混物拉伸强度稳定在 30 MPa 左右,断裂伸长率由116.1% 增至 276.1% ,显著高于 PBAT/ PLA 体系的 15.6% ;透光率曲线呈现透光性时的波长逐渐降低,而 PBAT/ PLA在 400~ 780 nm 波长内均不透光;水蒸气渗透系数(PH2O )由 1.23×10-13 g·cm/ (cm2·s·Pa)降至 1.18×10-13g·cm/ (cm2·s·Pa),氧气渗透系数(PO2)由 2.32×10-14 cm3·cm/ (cm2·s·Pa)降至 2.18×10-14cm3·cm/ ( cm2·s·Pa),低于 PBAT/ PLA,气体阻隔性能提升。

    Abstract:

    To develop novel blend materials combining the performance advantages of poly(butylene adipateco-terephthalate) ( PBAT) and polylactic acid ( PLA), in this study, the block polymer PBAT-b-PLA was introduced into the PBAT / PLA blend system, forming the ternary blend PBAT / PBAT-b-PLA / PLA. The compatibilizing effect of the block copolymer on the blend and its impact on mechanical, optical, and gas barrier properties were systematically investigated. Differential scanning calorimetry and scanning electron microscopy analyses reveal that PBAT-b-PLA significantly enhances the compatibility between PBAT and PLA. The dispersed phase size and the difference of glass transition temperatures ( ΔTg) between the two phases decreases from 5712 nm and 94.22 ℃ in the PBAT / PLA blend to less than 1200 nm and 94.00 ℃, respectively. The dispersed phase size decreases as the number average molecular weight of PBAT-b-PLA is reduced; when the molecular weight decreases from 8.5 × 104 to 3.0 × 104, the dispersed phase size decreases from 1186 nm to 426 nm. The compatibilization by PBAT-b-PLA endows the ternary blend PBAT / PBAT-b-PLA / PLA with superior properties compared to PBAT / PLA, and these properties vary with the molecular weight of PBAT-b-PLA. As the molecular weight decreases from 8.5×104 to 3.0×104, the tensile strength of the ternary blend remains stable at approximately 30 MPa, while the elongation at break increases from 116.1% to 276.1% —significantly higher than the 15.6% observed in PBAT / PLA. The onset wavelength for light transmission gradually decreases, whereas PBAT / PLA exhibits no transmittance in the visible light range ( 400 ~ 780 nm). The water vapor permeability coefficient (PH2O) decreases from 1.23 × 10-13 g·cm/ (cm2·s·Pa) to 1.18 × 10-13 g·cm/ (cm2·s·Pa), and the oxygen permeability coefficient (PO2) decreases from 2.32×10-14 cm3·cm/ (cm2·s·Pa) to 2.18×10-14 cm3·cm/ (cm2·s·Pa), both lower than those of PBAT / PLA, indicating enhanced gas barrier performance.

    参考文献
    相似文献
    引证文献
引用本文

张 涵, 曹继龙, 江 龙, 黄 云, 淡 宜.嵌段聚合物 PBAT-b-PLA 在共混物 PBAT/PBAT-b-PLA/PLA中的增容作用及对共混物性能的影响[J].高分子材料科学与工程,2026,42(6):70-77. Han Zhang, Jilong Cao, Long Jiang, Yun Huang, Yi Dan. Compatibilizing Effect of Block Polymer PBAT-b-PLA in PBAT/ PBAT-b-PLA / PLA Blends and Its Influence on Blend Properties[J]. Polymer Materials Science & Engineering,2026,42(6):70-77.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2026-10-24
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司