Preparation and Properties of Degradable and Flame-Retardant Epoxy Resin Based on Vanillin
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为提升环氧树脂的阻燃性和可降解性,文中以香草醛为主要原料合成了香草醛基环氧单体(Van-EP);以阻燃单元六氯环三磷腈为主要原料合成了六(4-氨基苯氧基)环三磷腈(HACP),将其作为阻燃剂兼固化剂,制备了交联密度高的香草醛基可降解阻燃环氧树脂(HVEP),研究了其固化行为、热稳定性、降解性能、力学和阻燃性能。通过非等温差示扫描量热法对HVEP 体系的固化行为进行了分析,采用自催化模型获得其固化动力学参数,发现拟合得到的曲线与实验曲线基本吻合,表明自催化模型在2.5~20 K / min 的升温速率范围内能较好地描述HVEP 体系的固化反应过程。通过外推法确定了体系的固化工艺:120 ℃ 固化2 h,150 ℃ 固化2 h。在该工艺条件下制备的HVEP 树脂的弯曲强度和冲击强度分别为153 MPa 和2.74 kJ / m2;其热稳定性与商用环氧树脂相当,其在1000 ℃ 时的残碳率高达48.4% 。HVEP 树脂具有优异的阻燃性能,其极限氧指数为28.4% ,垂直燃烧等级达到了UL-94 V-0 级。另外,HVEP树脂具有较好的降解性能,在0.2 mol / L 的HCl 溶液( THF / H2O 体积比8/ 2) 中,降解速率可达0.29 mg / ( mL·h)。HVEP 树脂分子链中含有环三磷腈和席夫碱阻燃结构单元,席夫碱结构同时具有可降解性,从而使其兼具良好的力学、阻燃和降解性能,对拓宽其应用领域具有重要意义。

    Abstract:

    To enhance the flame retardancy and degradability of epoxy resin, vanillin-based epoxy monomer (Van-EP ) was synthesized using vanillin as primary raw material. Additionally, hexa ( 4-acetylphenoxy ) cyclotriphosphazene (HACP) was synthesized from flame-retardant unit hexachlorocyclotriphosphazene to serve as flame retardant and curing agent, thereby preparing a highly cross-linked, degradable, and flame-retardant vanillin-based epoxy resin. The curing behavior, thermal stability, degradability, mechanical properties, and flame retardancy of the vanillin-based degradable flame-retardant epoxy resin ( HVEP ) were systematically investigated. Non-isothermal differential scanning calorimetry (DSC) was employed to analyze the curing kinetics of HVEP. The curing kinetics parameters were obtained using the self-catalytic model, and it is found that the fitted curve is in good agreement with the experimental curve. The results indicate that the autocatalytic model can accurately describe the curing process within heating rates of 2.5~20 K / min. The optimal curing conditions was determined by extrapolation method as follows:2 h at 120 ℃ followed by 2 h at 150 ℃ . The resulting HVEP resin exhibits a flexural strength of 153 MPa and an impact strength of 2.74 kJ / m2. The HVEP resin demonstrates comparable thermal stability to commercial epoxy resin (EP). However, it achieves a significantly higher char yield of 48.4% at 1000 ℃ . Furthermore, HVEP resin displays excellent flame retardancy with a limiting oxygen index (LOI) of 28.4% and achieves a UL-94 V-0 rating in the vertical burning test. In addition, the HVEP resin displays relatively good degradability, with a degradation rate reaching 0.29 mg / (mL·h) in a 0.2 mol / L HCl solution (V (THF) / V (H2O) = 8/ 2). The results indicate that the molecular chain of HVEP contains both cyclotriphosphazene and Schiff base structural units, which contribute to its flame retardancy. The Schiff base structure also imparts degradability, enabling HVEP to exhibit balanced mechanical, flame-retardant, and degradable properties. These findings are of significant importance for broadening its application fields.

    参考文献
    相似文献
    引证文献
引用本文

金昊晟, 郑 波, 颜 春, 祝颖丹, 刘 东, 徐海兵, 刘小青, 代金月.可降解阻燃香草醛基环氧树脂的制备及性能[J].高分子材料科学与工程,2026,42(7):110-120. Haosheng Jin, Bo Zheng, Chun Yan, Yingdan Zhu, Dong Liu, Haibing Xu, Xiaoqing Liu, Jinyue Dai. Preparation and Properties of Degradable and Flame-Retardant Epoxy Resin Based on Vanillin[J]. Polymer Materials Science & Engineering,2026,42(7):110-120.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2026-11-19
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司